The invention concerns films having a cling layer of an elastomeric
propylene-based polymer with a low heat of fusion derived from isotactic
propylene type crystallinity, as determined by DSC of less than 40 J/g,
optionally blended with a crystalline isotactic propylene derived polymer
having a heat of fusion over 70 J/g and/or a melting point of at least
120.degree. C. as determined by DSC, and a non-cling layer of a
polyolefin. The cling layer may contain other components such as
crystalline polypropylene.