The C-type nickel base alloys of the type containing significant amounts of chromium (about 16 to 25%) and molybdenum (about 12 to 18%) may be improved by adding small but critical amounts of copper (about 1 to 3.5%) which their general corrosion resistance to a wide range of both oxidizing and non-oxidizing industrial media.

 