A process for producing a positive electrode active material for a
nonaqueous secondary battery comprising the steps of: dissolving compounds
capable of providing lithium ions, nickel ions and optionally ions of at
least one element selected from the group consisting of transition
metals,-3B-group elements, 4B-group elements and 5B-group elements in a
buffer solution containing at least lithium ions, thereby to prepare a
starting aqueous solution; adding an oxalic acid to the starting aqueous
solution to form a precipitate of oxalates of said ions and separating the
precipitate; calcining the resulting precipitate to produce LiNI.sub.1-x
M.sub.x O.sub.2, wherein 0.ltoreq.X<0.5 and M is at least one element
selected from the group consisting of the transition metals, 3B-group
elements, 4B-group elements and 5B-group elements; and re-using a residual
liquid after the precipitate is separated for preparing the starting
aqueous solution.
Un procedimento per produrre un materiale attivo dell'elettrodo positivo per una batteria secondaria non acquosa che contiene i punti: residui di dissoluzione capaci di fornire gli ioni del litio, gli ioni del nichel e facoltativamente gli ioni almeno di un elemento scelto dai metalli consistenti di transizione del gruppo, gli elementi di -3B-group, gli elementi 4B-group e gli elementi 5B-group in una soluzione tampone che contiene almeno gli ioni del litio, quindi per preparare una soluzione acquosa iniziante; aggiungendo un acido ossalico alla soluzione acquosa iniziante per formare un precipitato degli ossalati degli ioni detti e di separazione del precipitato; calcinando il precipitato risultante per produrre LiNI.sub.1-x M.sub.x O.sub.2, in cui 0.ltoreq.X