A method of consolidating metal powder to form an object that includes pressing the powder into a preform, and preheating the preform to elevated temperature; providing flowable pressure transmitting particles and transmitting microwaves into the particles to heat same, and providing a bed of the flowable and heated pressure transmitting particles; positioning the preform in such relation to the bed that the particles substantially encompass the perform; and pressurizing the bed to compress the particles and cause pressure transmission to the preform, thereby to consolidate the preform into a desired object shape, the powder of step a) consisting essentially of at least two of the following: W, Ni, Fe, Co, manganese and titanium, and preferably at least three of same.

Метод консолидировать порошок металла для того чтобы сформировать предмет вклюает отжимать порошок в preform, и подогревать preform к повышенной температуре; предусматривающ, что частицы flowable давления передавая и передающ микроволны в частицы нагрел такие же, и обеспечивать кровать flowable и нагретых частиц давления передавая; располагать preform в таком отношении к кровати что частицы существенн включают выполнять; и надувающ кровать для того чтобы обжать частицы и причинить передачу давления к preform, таким образом для того чтобы консолидировать preform в заданную форму предмета, порошок шага a) состоя необходимо по крайней мере 2 из following: Ш, ni, fe, co, маргаец и титан, и предпочтительн по крайней мере 3 таких же.

 
Web www.patentalert.com

< (none)

< Disk drive assembly with improved securing and releasing mechanism

> Electric gun

> (none)

~ 00029