The present invention comprises an alum/rosin composition for internally sizing paper which is useful in any papermaking furnish with moderate to high hardness, as well as methods for preparing such alum/rosin composition. Employing the invention alum/rosin composition of an alum to rosin ratio of 1-3:1, respectively, and of a mean particle diameter of no greater than 10 microns, results in sizing of improved efficiency. In the preparation of the invention sizing composition, the pre-reacting of either neat or solutions of alum and rosin before introducing the mixture into the papermaking furnish, allows the alum to be free to react with the rosin size without any competition from other cations in the furnish.

Присытствыющий вымысел состоит из состава alum/rosin для внутренне определяя размер бумаги полезна в любом papermaking обеспечивает с вмеру к высокой твердости, также,как методы для подготовлять такой состав alum/rosin. Использовать состав вымысла alum/rosin квасцов к коэффициенту канифоли 1-3:1, соответственно, и среднего диаметра частицы of no greater than 10 микронов, приводит к в загрунтовке улучшенной эффективности. В подготовке состава загрунтовкы вымысла, пре-reagirovat6 или опрятного или разрешений квасцов и канифоли перед вводить смесь в papermaking поставляет, позволяет квасцы быть свободно прореагировать с размером канифоли без любой конкуренции от других катионов в обеспечении.

 
Web www.patentalert.com

< (none)

< Hair styling oil

> Method of making paper from aldehyde modified cellulose pulp with selected additives

> (none)

~ 00032