To provide a method for producing a molded crystalline resin article which
enables a higher crystallization degree and to mass-produce the molded
crystalline resin articles. The method comprises molding a molded resin
article from a thermoplastic resin containing a crystalline resin followed
by performing a heating process to obtain a molded crystalline resin
article having a surface layer whose crystallization index is 0.9 or
higher when determined by IR spectrometry. It is preferable that the
temperature of the heating process is within the range of 20.degree. C.
lower than the crystallization temperature of the molded resin article to
30.degree. C. higher than the crystalline temperature, and that the
crystalline resin is a polypropylene resin.
Pour fournir une méthode pour produire un article cristallin moulé de résine qui permet un degré plus élevé de cristallisation et pour produire les articles cristallins moulés de résine. La méthode comporte mouler un article moulé de résine d'une résine thermoplastique contenant une résine cristalline suivie d'effectuer un processus de chauffage pour obtenir un article cristallin moulé de résine ayant une couche extérieure dont l'index de cristallisation est 0.9 ou plus haut une fois déterminé par spectrométrie d'IR. Il est préférable que la température du processus de chauffage soit dans la marge de 20.degree. C. inférieur la température de cristallisation de l'article moulé de résine à 30.degree. Le C. plus haut que la température cristalline, et ce la résine cristalline est une résine de polypropylène.