A platinum colloid is formed by reducing platinum ions by agitating a
treatment solution, while controlling temperature of the treatment
solution under a reductive atmospheric condition. The solution contains
one part of capacity of a platinum chloride acid solution, 400 to 500
parts of capacity of water, a non-ion based surface-active agent in an
amount of 0.2 to 2 times with respect to an amount of the platinum
chloride acid solution, a reducing agent in an amount of 40 to 60 times
with respect to the amount of the platinum cloride acid solution, and a Ph
compensating agent in an amount of 10 to 30 times with respect to the
amount of the platinum chloride acid solution if the concentration thereof
is 5%, to thereby adjust pH of the treatment solution to neutral or weak
alkalinity.
Ein Platinkolloid wird gebildet, indem man Platinionen verringert, indem man aufregt eine Behandlunglösung, beim Steuern der Temperatur der Behandlunglösung unter einer vermindernden atmosphärischen Bedingung. Die Lösung enthält ein Teil Kapazität einer Platinchlorverbindung sauren Lösung, 400 bis 500 Teile Kapazität des Wassers, ein Nichtion gegründetes oberflächenaktives Mittel in einer Menge von 0.2 bis 2mal in Bezug auf eine Menge der Platinchlorverbindung sauren Lösung, ein Reduktionsmittel in einer Menge von 40 bis 60mal in Bezug auf die Menge der Platin cloride sauren Lösung und ein pH ausgleichendes Mittel in einer Menge von 10 bis 30mal in Bezug auf die Menge der Platinchlorverbindung sauren Lösung, wenn die Konzentration davon 5% ist, pH der Behandlunglösung auf Null- oder schwache Alkalinität dadurch zu justieren.