A multi-ply composite container for consumer products with at least one
region of weakened strength and method for manufacturing same is provided.
The composite container includes a multi-ply composite tube having a
tubular body ply, a liner ply adhered to the inner surface of the tubular
body ply and a label ply adhered to the outer surface of the body ply. The
composite container also includes at least one circumferential score line
in the multi-ply composite tube through the label ply and the body ply.
The container and method overcome limitations imposed by conventional
composite containers by providing a composite container which provides for
easy opening, better consumer access, resealability, storage for left over
food product, and easier consumer recycling.
Een multi-ply samengestelde container voor verbruiksgoederen met minstens één gebied van verzwakte sterkte en methode voor productiezelfde wordt verstrekt. De samengestelde container omvat een multi-ply samengestelde buis die een tubulaire lichaamsvouw heeft, hing een voeringsvouw de binnenoppervlakte van de tubulaire lichaamsvouw aan en een etiketvouw hing de buitenoppervlakte van de lichaamsvouw aan. De samengestelde container omvat ook minstens één perifere scorelijn in de multi-ply samengestelde buis door de etiketvouw en de lichaamsvouw. De container en de methode overwinnen beperkingen die door conventionele samengestelde containers door een samengestelde container worden opgelegd te verstrekken die het gemakkelijke openen, betere toegang van de consument, resealability, opslag voor linkerzijde over voedingsmiddelen, en gemakkelijker recycling van de consument voorziet.