A method for tissue augmentation in a mammal is provided having injecting a
polymer at a tissue site in need of augmentation and having a tissue
temperature, the polymer having repeating peptide monomeric units selected
from the group consisting of nonapeptide, pentapeptide and tetrapeptide
monomeric units, wherein the monomeric units form a series of .beta.-turns
separated by dynamic bridging segments suspended between the .beta.-turns,
wherein the polymer has an inverse temperature transition T.sub.t less
than the tissue temperature, and wherein the polymer is injected as a
water solution at coacervate concentration in the substantial absence of
additional water. A kit containing the injectable bioelastic polymer and a
syringe is also provided.
Un método para el aumento del tejido fino en un mamífero se proporciona teniendo inyectar un polímero en un sitio del tejido fino en la necesidad del aumento y tener una temperatura del tejido fino, el polímero que tiene repetición de las unidades monomeric del peptide seleccionadas del nonapeptide que consiste en del grupo, el pentapeptide y unidades monomeric del tetrapeptide, en donde las unidades monomeric forman una serie de beta.-dan vuelta separado por los segmentos que tienden un puente sobre dinámicos suspendidos entre beta.-dan vuelta, en donde el polímero tiene una transición inversa T.sub.t de la temperatura menos que la temperatura del tejido fino, y en donde el polímero se inyecta como solución del agua en la concentración del coacervate en la ausencia substancial del agua adicional. Un kit que contiene el polímero bioelastic inyectable y una jeringuilla también se proporciona.