Disclosed is a two-step method of making soft, high refractive index,
acrylic ophthalmic device materials. In the first step, a copolymer
containing pendant oxirane groups is formed by copolymerizing one or more
aryl acrylic hydrophobic monomers with one or more compounds of the
formula
##STR1##
wherein
X is H or CH.sub.3 ; and
n is 1-4.
In the second step, the copolymer containing pendant oxirane groups formed
in the first step is reacted with a compound of the formula
W--T--H
wherein
W is H, CH.sub.3 (CH.sub.2).sub.a, or Z(OCH.sub.2 CH.sub.2).sub.b ;
a is 0-3;
b is 1-5;
Z is H, or CH.sub.3 (CH.sub.2).sub.p ;
p is 0-3; and
T is O, NH, S; provided that if T.noteq.O, then W.noteq.H.
È rilevato un metodo di fabbricazione in due tappe morbido, l'alto indice di rifrazione, materiali oftalmici acrilici del dispositivo. Al primo punto, un copolimero che contiene i gruppi pendant dell'oxirane è costituito dal copolymerizing uno o più monomeri idrofobi acrilici arilici con uno o più residui del ## del ## STR1 di formula in cui la X è H o CH.sub.3; e la n è 1-4. Al secondo punto, il copolimero che contiene i gruppi pendant dell'oxirane formati al primo punto è reagito con un residuo della formula il W -- t -- h in cui il W è H, CH.sub.3 (CH.sub.2).sub.a, o Z(OCH.sub.2 CH.sub.2).sub.b; la a è 0-3; la b è 1-5; La Z è H, o CH.sub.3 (CH.sub.2).sub.p; la p è 0-3; e la T è O, il NH, S; a condizione che se T.noteq.O, allora W.noteq.H.