The invention provides a method of making an analogue of .beta."-alumina,
the analogue having a layered .beta."-alumina spinel-type structure in
which ate least some of the Na ions in the layers of Na ions separated by
layers of Al and O ions in said .beta."-alumina spinel-type structure are
replaced by substitute metal cations. The substitute metal cations are
mono-, d- and/or trivalent. The method comprises dispersing in a boehmite
having a well developed and highly ordered crystal structure at least one
oxide of the substitute metal cations or a precursor thereof to form a
starting mixture, and heating the mixture to a conversion temperature at
which it is converted to the analogue.
Die Erfindung liefert eine Produktionsmethode eine Entsprechung von Beta."tonerde, die Entsprechung, die eine überlagerte Beta."tonerde Spinelart Struktur hat, in der wenige einige der Na Ionen in den Schichten der Na Ionen aß, die durch Schichten Al getrennt wurden und O Ionen in besagter Beta."tonerde Spinelart Struktur durch Ersatzmetallkationen ersetzt werden. Die Ersatzmetallkationen sind- -, d und/oder dreiwertiges mono. Die Methode enthält das Zerstreuen in einem boehmite, das einen Brunnen sich entwickeln läßt und bestellte in hohem Grade Kristallstruktur mindestens ein Oxid der Ersatzmetallkationen oder des Vorläufers davon, um eine beginnende Mischung und das Heizen der Mischung zu einer Umwandlung Temperatur zu bilden, bei der sie in die Entsprechung umgewandelt wird.