The present invention relates to a method for determining concentration of
brightener and leveler contained in an aqueous acid metal electroplating
solution, by firstly determining the concentration of the brightener at a
first set of measurement conditions, and secondly determining the
concentration of the leveler at a second set of measurement conditions,
provided that the first set of measurement conditions differ from the
second set of measurement conditions on the rotation speed of a rotating
disc electrode used for measuring plating potential of said aqueous acid
metal electroplating solution, and optionally, the electroplating duration
at which the plating potential of said aqueous acid metal electroplating
solution is measured, provided that the first rotation speed is lower than
the second rotation speed, and that the first electroplating duration is
shorter than the second electroplating duration.
Η παρούσα εφεύρεση αφορά μια μέθοδο για τη συγκέντρωση brightener και leveler σε ένα υδάτινο όξινο μέταλλο τη λύση ηλεκτρολυτικής επιμετάλλωσης, με αρχικά τον καθορισμό της συγκέντρωσης brightener σε ένα πρώτο σύνολο όρων μέτρησης, και αφετέρου τον καθορισμό της συγκέντρωσης του leveler σε ένα δεύτερο σύνολο όρων μέτρησης, υπό τον όρο ότι το πρώτο σύνολο όρων μέτρησης διαφέρει από το δεύτερο σύνολο όρων μέτρησης στην ταχύτητα περιστροφής ενός περιστρεφόμενου ηλεκτροδίου δίσκων που χρησιμοποιείται για τη μέτρηση της δυνατότητας επένδυσης της εν λόγω υδάτινης όξινης λύσης ηλεκτρολυτικής επιμετάλλωσης μετάλλων, και προαιρετικά, η διάρκεια ηλεκτρολυτικής επιμετάλλωσης στην οποία η δυνατότητα επένδυσης της εν λόγω υδάτινης όξινης λύσης ηλεκτρολυτικής επιμετάλλωσης μετάλλων μετριέται, υπό τον όρο ότι η πρώτη ταχύτητα περιστροφής είναι ταχύτητα, και ότι η πρώτη διάρκεια ηλεκτρολυτικής επιμετάλλωσης είναι πιό σύντομη από τη δεύτερη διάρκεια ηλεκτρολυτικής επιμετάλλωσης.