Recovery of PEM fuel cell performance is achieved by evacuating (61, 62) or
by flowing water absorbing gas (46) through, or both, the fuel flow field
(12, 13, 19, 20), the air flow field (25, 26, 30, 31), and the water flow
field (36, 39), while resistance of the individual cells, or of the fuel
cell stack, is measured; the dry out process is continued until the
resistance of the cells (or the resistance per cell, measured across the
fuel cell stack as a whole), has increased by at least 5 to 1 (preferably
10 to 1) over the normal resistance of the cells. The water absorbing gas
may be air (23) or nitrogen (47); it may be at ambient temperature or
heated (50).
Il recupero delle prestazioni delle cellule di combustibile del PEM è realizzato evacuando (61, 62) o dal gas assorbente fluente dell'acqua (46) attraverso, o entrambi, il campo di flusso del combustibile (12, 13, 19, 20), il campo di corrente d'aria (25, 26, 30, 31) ed il campo di flusso dell'acqua (36, 39), mentre resistenza di diverse cellule, o della pila delle cellule di combustibile, sono misurati; il processo di asciug è continuato fino alla resistenza delle cellule (o alla resistenza per la cellula, misurata attraverso la pila delle cellule di combustibile nell'insieme), è aumentato almeno di 5 - 1 (preferibilmente 10 - 1) eccedenza la resistenza normale delle cellule. Il gas assorbente dell'acqua può essere aria (23) o azoto (47); può essere alla temperatura ambientale o ha riscaldato (50).