The present invention concerns high-stiffness polymer composition and a
process for producing a polymer composition by nucleated with a polymeric
nucleating agent containing vinyl compound units. The method comprises
modifying a catalyst by polymerizing a vinyl compound in the presence of
said catalyst and a strongly coordinating donor in a medium, which does
not essentially dissolve the polymerized vinyl compound, and by continuing
the polymerization of the vinyl compound until the concentration of
unreacted vinyl compounds is less than about 0.5 wt-%. The thus obtained
modified catalyst composition is used for polymerizing propylene
optionally together with comonomers in the presence of said modified
catalyst composition. Modification of the catalyst according to the
present invention will reduce production costs and provide highly reliable
catalyst activity and polymers of high stiffness.
Die anwesende Erfindung betrifft Hochsteifheit Polymer-Plastik Aufbau und einen Prozeß für das Produzieren eines Polymer-Plastik Aufbaus durch kernhaltiges mit einem polymerischen nucleating Mittel, das Vinylzusammengesetzte Maßeinheiten enthält. Die Methode enthält das Ändern eines Katalysators, indem sie ein Vinylmittel in Anwesenheit des besagten Katalysators und eines stark koordinierenspenders in einem Mittel polymerisiert, das nicht im Wesentlichen das polymerisierte Vinylmittel auflöst, und indem sie die Polymerisierung des Vinylmittels fortsetzt, bis die Konzentration der ohne Reaktion Vinylmittel kleiner als ungefähr 0.5 wt-% ist-. Der folglich erhaltene geänderte Katalysatoraufbau wird für Propylen beliebig polymerisieren zusammen mit Comonomeren in Anwesenheit des besagten geänderten Katalysatoraufbaus benutzt. Änderung des Katalysators entsprechend der anwesenden Erfindung verringert Produktion Kosten und liefert in hohem Grade zuverlässige Katalysatortätigkeit und Polymer-Plastiken der hohen Steifheit.