A high molecular weight, medium density polyethylene (HMW, MDPE) is
disclosed. The polyethylene comprises from about 85 to about 98 wt % of
recurring units of ethylene and about 2 to about 15 wt % of a
C.sub.3-C.sub.10 .alpha.-olefin. It has a density from about 0.92 to about
0.944 g/cc, a melt index MI.sub.2 from about 0.01 to about 0.5 dg/min, and
a melt flow ratio MFR from about 50 to about 300. It has a multimodal
molecular weight distribution comprising a high molecular weight component
and a low molecular weight component. The low molecular weight component
has an MI.sub.2 from about 50 to about 600 dg/min and a density from about
0.94 to about 0.97 g/cc. A process for making the medium density
polyethylene is also disclosed. The process uses a Ziegler catalyst and
applies multiple reaction zones.
Se divulga un alto peso molecular, el polietileno medio de la densidad (HMW, MDPE). El polietileno abarca de cerca de 85 a cerca de 98 pesos % de unidades que se repiten del etileno y de cerca de 2 a cerca de 15 pesos % de un alpha.-alpha.-olefin C.sub.3-C.sub.10. Tiene una densidad de cerca de 0.92 a cerca de 0.944 g/cc, un índice MI.sub.2 del derretimiento de cerca de 0.01 a cerca de 0.5 dg/min, y un cociente MFR del flujo del derretimiento de cerca de 50 a cerca de 300. Tiene una distribución multimodal del peso molecular el abarcar de un alto componente del peso molecular y de un componente bajo del peso molecular. El componente bajo del peso molecular tiene un MI.sub.2 de cerca de 50 a cerca de 600 dg/min y una densidad de cerca de 0.94 a cerca de 0.97 g/cc. Un proceso para hacer el polietileno medio de la densidad también se divulga. El proceso utiliza un catalizador de Ziegler y aplica zonas múltiples de la reacción.