Methods and devices are provided for enhancing corrosion of an electrode in
a biocompatible fluid. The method comprises (1) placing a primary
electrode and a counter electrode in an electroconductive biocompatible
fluid to form an electrochemical cell; and (2) applying a time-varying
potential, through the electrochemical cell, to the primary electrode. In
a preferred embodiment, the primary electrode is metal and comprises a
reservoir cap of a microchip device for the release of molecules or
exposure of device reservoir contents. The potential preferably is
characterized by a waveform having a maximum potential effectively anodic
to meet or exceed the corrosion potential of the primary electrode. Also,
the minimum potential preferably is effectively cathodic to be below the
value where re-deposition of metal ions on the metal electrode can
substantially occur, thereby corroding the metal electrode.
I metodi ed i dispositivi sono forniti per l'aumento della corrosione di un elettrodo in un liquido biocompatible. Il metodo contiene (1) disponendo un elettrodo primario e un controelettrodo in un liquido biocompatible elettroconduttore per formare una cellula elettrochimica; e (2) applicando un potenziale divariazione, attraverso la cellula elettrochimica, all'elettrodo primario. In un metodo di realizzazione preferito, l'elettrodo primario è metallo e contiene una protezione del serbatoio un dispositivo del microchip per il rilascio delle molecole o l'esposizione del soddisfare del serbatoio del dispositivo. Il potenziale è caratterizzato preferibilmente efficacemente da una forma d'onda che ha un potenziale massimo anodico per venire a contatto o eccedere del potenziale di corrosione dell'elettrodo primario. Inoltre, il potenziale minimo è preferibilmente efficacemente catodico essere sotto il valore dove il re-deposito degli ioni del metallo sull'elettrodo del metallo può accadere sostanzialmente, quindi corrodente l'elettrodo del metallo.