The present invention relates to a method for fabricating an integrally
bladed rotor which comprises providing a hub section, preferably formed
from a titanium based alloy, and welding an airfoil, also preferably
formed from a titanium based alloy, to the hub section. The method further
comprises partially aging and cooling the hub section prior to welding and
aging the airfoil and the weld joint between the airfoil and the hub
section subsequent to welding. The post welding aging step is preferably
carried out using a novel encapsulated local airfoil heating device having
a plurality of heating elements woven into a jacket made from a high
temperature cloth material. The method of the present invention may also
be used to repair integrally bladed rotors.
La présente invention concerne une méthode pour fabriquer un rotor intègralement à lames qui comporte fournir une section de moyeu, de préférence formée d'un alliage basé titanique, et de souder une aile, de préférence formée également d'un alliage basé titanique, à la section de moyeu. La méthode autre comporte partiellement vieillir et refroidir la section de moyeu avant la soudure et le vieillissement l'aile et le joint de soudure entre l'aile et la section de moyeu suivantes à la soudure. L'étape de vieillissement de soudure de poteau est de préférence effectuée à l'aide d'un dispositif de chauffage local encapsulé par roman d'aile ayant une pluralité d'éléments de chauffe tissés dans une veste faite à partir d'un matériel à hautes températures de tissu. La méthode de la présente invention peut également être employée pour réparer intègralement les rotors à lames.