An electrochemical cell having a cathode containing an expanded graphite as
an electrically conductive carbon material. To provide enhanced service
performance in the cell, the expanded graphite has a kerosene absorption
in the range of 2.2 to 3.5 ml/g, an average particle size of 17 to 32
micrometers, a d.sub.90 value of 40 to 85 micrometers, and an average
surface area-to-mass ratio of at least 18 m.sup.2 /g. A method is also
provided for determining an optimum expanded graphite including the steps
of measuring physical characteristics of the expanded graphite determining
the performance of a cell containing the expanded graphite in the positive
electrode, and determining the optimum expanded graphite for use in the
cell.
Uma pilha eletroquímica que tem um cátodo conter uma grafita expandida como um material eletricamente condutor do carbono. Para fornecer o desempenho do serviço realçado na pilha, a grafita expandida tem um absorption do querosene na escala de 2.2 a 3.5 ml/g, de um tamanho de partícula médio de 17 a 32 micrômetros, de um valor d.sub.90 de 40 a 85 micrômetros, e de uma relação de superfície média da área-à-massa ao menos de 18 m.sup.2 /g. Um método é fornecido também determinando uma grafita expandida a melhor including as etapas de medir características físicas da grafita expandida que determina o desempenho de uma pilha que contem a grafita expandida no elétrodo positivo, e determinando a grafita expandida a melhor para o uso na pilha.