The present invention provides a process of reducing the amount of
fluorinated emulsifier in an aqueous fluoropolymer dispersion by
contacting the aqueous fluoropolymer dispersion with an anion exchange
resin in a non-fixed resin bed, the process comprising:
(a) mixing the aqueous fluoropolymer dispersion with an effective amount of
a surfactant so as to stabilize the fluoropolymer dispersion while being
contacted with the anion exchange resin;
(b) contacting the aqueous fluoropolyrner dispersion with an anion exchange
resin by agitating the aqueous fluoropolymer dispersion with an effective
amount of anion exchange resin for a time of less than 4 hours to reduce
the amount of fluorinated emulsifier in the aqueous fluoropolymer
dispersion to a desired level; and
(c) separating the anion exchange resin from the aqueous fluoropolymer
dispersion.
De onderhavige uitvinding voorziet een proces om de hoeveelheid fluorinated emulgator in een waterige fluoropolymer verspreiding te verminderen door de waterige fluoropolymer verspreiding te contacteren van een hars van de anionuitwisseling in een niet-vast harsbed, het proces bestaand uit: (a) het mengen van de waterige fluoropolymer verspreiding met een efficiƫnte hoeveelheid capillair-actieve stof om de fluoropolymer verspreiding te stabiliseren terwijl wordt gecontacteerd met de hars van de anionuitwisseling; (b) contacterend de waterige fluoropolyrnerverspreiding met een hars van de anionuitwisseling door de waterige fluoropolymer verspreiding met een efficiƫnte hoeveelheid hars van de anionuitwisseling voor een tijd van minder te ageren dan 4 uren om de hoeveelheid fluorinated emulgator in de waterige fluoropolymer verspreiding op een gewenst niveau te verminderen; en (c) scheidend de hars van de anionuitwisseling van de waterige fluoropolymer verspreiding.