Microfabrication of organic optical elements

   
   

Method of fabricating an optical element. A photodefinable composition is provided that includes (i) a hydrophobic, photodefinable polymer, said photodefinable polymer having a glass transition temperature in the cured state of at least about 80.degree. C.; and (ii) a multiphoton photoinitiator system comprising at least one multiphoton photosensitizer and preferably at least one phtoinitiator that is capable of being photosensitized by the photosensitizer. One or more portions of the composition are imagewise exposed to the electromagnetic energy under conditions effective to photodefinably form at least a portion of a three-dimensional optical element.

Метод изготовлять оптически элемент. Photodefinable состав provided that вклюает (i) гидродобный, photodefinable полимер, сказанный photodefinable полимер имея температуру стеклянного перехода в вылеченном положении по крайней мере около 80.degree. C; и (ii) система photoinitiator multiphoton состоя из по крайней мере одного фотосенсибилизатора multiphoton и предпочтительн по крайней мере одного phtoinitiator способно быть photosensitized фотосенсибилизатором. One or more части состава imagewise подвергаются действию к электромагнитной энергии под условиями эффективными photodefinably для того чтобы сформировать по крайней мере часть трехмерного оптически элемента.

 
Web www.patentalert.com

< Surface coating spatially controlled patterns

< Methods for producing composite nanoparticles

> Process for preparing hydro-desulfurization catalyst

> Antisense modulation of damage-specific DNA binding protein 1, p127 expression

~ 00162