The present invention provides improved well cementing methods for use in cold environment, where the circulating temperature of the cement is typically within the range of 5 to 20 C. The improved well cementing methods include forming compositions that are essentially comprised of an aqueous fluid, a hydraulic cement binder and a set-accelerating admixture comprising an alkali or alkaline earth metal nitrate and an alkali or alkaline earth metal nitrite.

 