A paper product is described that includes a paper substrate having a first surface and a second surface; a coating layer provided on the first surface of the paper substrate, the coating layer comprising a binder component and a pigment component, wherein the weight ratio the binder component to the pigment component is between about 0.25:1 to about 1:1; and wherein the paper product exhibits a gloss of at least about 20 to 75 according to TAPPI T480 om-92, a Print-surf roughness of at least about 0.5 to 2.5 according to TAPPI T555 pm-94, and a density of at least about 12 to 18 according to TAPPI T410 om-93 and TAPPI T411 om-89. A method for manufacturing a paper product is provided.

 