The present invention provides a process for producing a polyester from a polyester composition comprising at least about 1 wt. % wollastonite, based on the total weight of the polyester composition, wherein the wollastonite is added at a temperature of about 240.degree. C. or less. The present invention further provides a process for producing a polyester from a polyester composition comprising at least about 1 wt. % wollastonite, based on the total weight of the polyester composition, and about 0.01 wt. % other filler, based on total weight of the polyester composition, wherein the wollastonite is added at a temperature of about 240.degree. C. or less. The invention is further directed to polyester products produced by said process and the shaped articles formed therefrom.

 