The present invention provides an austenitic stainless steel tube with a uniform fine grained structure of regular grains, which is not changed to a coarse structure and the steam oxidation resistance is maintained even if the tube is subjected to a high temperature reheating during welding and high temperature bending working. The austenitic stainless steel tube consists of, by mass %, C: 0.03-0.12%, Si: 0.1-0.9%, Mn: 0.1-2%, Cr: 15-22%, Ni: 8-15%, Ti: 0.002-0.05%, Nb: 0.3-1.5%, sol. Al: 0.0005-0.03%, N: 0.005-0.2% and O (oxygen): 0.001-0.008%, and the balance Fe and impurities, the austenitic stainless steel tube having austenitic grain size number of 7 or more and a mixed grain ratio of preferably 10% or less.

 
Web www.patentalert.com

< Hydrogen storage metal alloy, method for absorption and release of hydrogen using the said alloy and hydrogen fuel battery using the said method

< Rare earth magnet alloy ingot, manufacturing method for the same, R-T-B type magnet alloy ingot, R-T-B type magnet, R-T-B type bonded magnet, R-T-B type exchange spring magnet alloy ingot, R-T-B type exchange spring magnet, and R-T-B type exchange spring bonded magnet

> Iron-nickel alloy material for shadow mask with excellent suitability for etching

> Titanium material superior in upset-forgeability and method of producing the same

~ 00247