A method of manufacturing a glazing panel having a solar factor (FS) of less
than
70% and being composed of a vitreous substrate and a tin/antimony oxide coating
layer provided on the vitreous substrate and having a Sb/Sn molar ratio ranging
from 0.01 to 0.5, preferable 0.03 to 0.5, the method including the steps of providing
reactants in gaseous phase which comprise tin and antimony compounds, which are
present in an amount effective to form the tin/antimony oxide coating layer; and
forming the tin/antimony oxide coating layer pyrolytically on the vitreous substrate
from the reactants in gaseous phase to provide the glazing panel having a solar
factor (FS) of less than 70%.