The first embodiment is a support for a lithographic printing plate, wherein
the surface area ratios obtained from three-dimensional data by use of an atomic
force microscope meets the following requirements (1-i) to (1-iii).
The second embodiment is a support for a lithographic printing plate, wherein
the aforementioned surface area ratios and a steepness meets the following requirements
(2-i) to (2-ii).
The third embodiment is a support for a lithographic printing plate, wherein
the aforementioned surface area ratios meets the following requirements (4-i) to (4-iii).
- (1-i) a surface area ratio S50(50) is 20 to 90%,
- (1-ii) a surface area ratio S50(2-50) is 1 to 30%, and
- (1-iii) a surface area ratio S50(0.2-2) is 5 to 40%,
- (2-i) a surface area ratio S50(50) is 30 to 60%, and
- (2-ii) a steepness a4550(0.2-2) is 5 to 40%,
- (4-i) a surface area ratio S5(5) is 20 to 90%,
- (4-ii) a surface area ratio S5(0.2-5) is 5 to 40%, and
- (4-iii) A surface area ratio S5(0.02-0.2) is 15 to 70%.
|
|
|