Methods of creating a stable slurry of coated particulates wherein the
slurry is capable of being stored for at least 2 hours before use
comprising the steps of: providing resin coated particulates wherein the
resin comprises a resin that does not completely cure unless it is at
least one of exposed to a temperature above about 175.degree. F. or
exposed to an external catalyst; and, substantially suspending the resin
coated particulates in a servicing fluid to create a stable resin coated
particulate slurry. Methods of creating a stable slurry of coated
particulates wherein the slurry is capable of being stored for at least 2
hours before use comprising the steps of: providing tackifier coated
particulates; and, substantially suspending the tackifier coated
particulates in a servicing fluid to create a tackifier coated
particulate slurry.