A method of providing a resistance to oxidation of Nickel at high
temperatures by combining Ni powder with five percent Pt resinate, and
heating the same to a temperature of 500.degree. C. to 1300.degree. C.
Electro-conductive components serving as electrodes and the like comprise
a Ni/Pt powder subjected to temperatures of between 500.degree. C. and
the respective melting points of Ni and Pt.