A method of servicing a wellbore, comprising preparing a sealant
composition comprising a crosslinkable material, a crosslinking agent, a
fluid loss control additive, and water, placing the sealant composition
in a permeable zone in the wellbore, and allowing the sealant composition
to set. A method of servicing a wellbore, comprising preparing a sealant
composition by combining a crosslinkable material, a crosslinking agent,
a fluid loss control additive, water, and a cement, wherein an amount of
the cement is reduced to an effective amount to increase a gel time of
the sealant composition to greater than or equal to about 4 hours when
the sealant composition is exposed to ambient temperatures in the
wellbore, placing the sealant composition in a permeable zone in the
wellbore, and allowing the sealant composition to gel.