A PDP resin sheet 11 capable of transmitting a rectilinear light is
prepared by alternately arranging a transparent section 12 and a dark
section 13 in the direction of the sheet surface. The transparent section
12 and the dark section 13 may be formed perpendicular or inclined to the
sheet surface, respectively. In the sheet 11, the thickness T of the
sheet may be about 0.12 to 0.25 mm, and the angle of the dark section 13
to the sheet surface may be about 70 to 90.degree.. In addition, the
ratio [P/T] of the periodical width P of the dark section relative to the
thickness T of the sheet may be about 1/1 to 1/2, and the ratio
[W.sub.1/W.sub.2] of the width W.sub.1 of the transparent section
relative to the width W.sub.2 of the dark section may be about 30/1 to
10/1. Soft resins constituting the transparent section and the dark
section may for example be an olefinic resin (particularly an
ethylene-vinyl ester copolymer). Such a PDP sheet ensures an image
display at high contrast even under a daylight environment, without
reducing a plasma display luminance.