A lithium-aluminosilicate glass ceramic is transformed by a suitable heat
treatment into a glass ceramic comprising at least 80 vol.-% of keatite
mixed crystals. This may be utilized for the preparation of optical or
mechanical high-precision parts having a high temperature resistance, a
good stability and compatibility with components consisting of metals
having a small coefficient of thermal expansion based on nickel and iron,
such as Invar.RTM..