It is an object of the present invention to eliminate a color deviation
possibly caused by a film formation failure in an organic layer of
organic EL devices, thereby improving product yield. A method of
manufacturing organic EL devices according to the invention comprises: a
pre-treating step for forming lower electrodes and the like on a
substrate, a film formation step to be performed after the pre-treating
step for forming on the lower electrodes an organic layer containing at
least an organic luminescent layer and also forming upper electrodes
thereon, and a sealing step to be performed after the film formation step
for sealing up the organic layer and the upper electrodes, characterized
in that an inspection step is performed after the pre-treating step but
before the formation of the upper electrodes.