Provided herein are methods that comprise: providing a foamed cement
composition that comprises a hydraulic cement, water, a gas, a foaming
and stabilizing surfactant, and a fluid loss control additive comprising
a copolymer; placing the foamed cement composition in a location to be
cemented; and allowing the foamed cement composition to set.