A coating comprsing a polymer (I)-containing coating component and
colloidal. silica (II) of 60 nm or less average particle diameter,
wherein 0.5 to 20 parts by mass, in terms of solid content, of colloidal
silica (II) is contained per 100 parts by mass of polymer (I) and wherein
the area of colloidal silica exposed from the surface of the coating
occupies 35% or more based on the coating surface. This coating exhibits
excellent antifouling performance and excels in transparency, weather
resistance, water resistance, and elongation degree.