A retardation film comprised of a single oriented polymer film, characterized in that the retardation at wavelengths of 450 nm and 550 nm satisfies the following formulae (1) and/or (2), and the water absorption is no greater than 1%. R(450)/R(550)<1 (1) K(450)/K(550)<1 (2) where R(450) and R(550) represent the in-plane retardation of the oriented polymer film at wavelengths of 450 nm and 550 nm, respectively, and K(450) and K(550) are the values calculated by K=[n.sub.z-(n.sub.x+n.sub.y)/2].times.d (where n.sub.x, n.sub.y and n.sub.z represent the three-dimensional refractive indexes of the oriented polymer film as the refractive indexes in the direction of the x-axis, y-axis and z-axis, respectively, and d represents the thickness of the film) for the oriented polymer film at a wavelength of 450 nm and 550 nm, respectively. There are provided laminated retardation films and liquid crystal display devices employing the retardation film.

 