Methods are provided that include a method of creating a stable slurry of coated particulates wherein the slurry is capable of being stored for at least 2 hours before use comprising the steps of: providing resin coated particulates wherein the resin comprises a resin that does not completely cure unless it is at least one of exposed to a temperature above about 175.degree. F. or exposed to an external catalyst; and, substantially suspending the resin coated particulates in a servicing fluid to create a stable resin coated particulate slurry. Methods are provided that include a method of creating a stable slurry of coated particulates wherein the slurry is capable of being stored for at least 2 hours before use comprising the steps of: providing tackifier coated particulates; and, substantially suspending the tackifier coated particulates in a servicing fluid to create a tackifier coated particulate slurry.

 