A method for producing a hydrorefining catalyst of the present invention
has a step of preparing an aluminum solution containing phosphorus in a
molar ratio of 0.001 to 0.05 with respect to aluminum; a step of
neutralizing the prepared aluminum solution to produce a pseudo-boehmite
powder; a step of forming the pseudo-boehmite powder followed by
performing calcination at a temperature of not less than 650.degree. C.
to obtain a carrier; and a step of carrying a hydrogenation-active metal
on the pseudo-boehmite powder or the carrier. The dispersion of the
concentration distribution of phosphorus in the carrier of the obtained
catalyst is within 10%. This method makes it possible to obtain the
hydrorefining catalyst which has a practically sufficient mechanical
strength and which has an excellent activity.