A low-k dielectric sacrificial material is formed within a microelectronic structure covered with a suitable porous or low density permeable material. At an appropriate time, the underlying sacrificial material is decomposed and diffused away through the overlying permeable material. As a result, at least one void is created, contributing to desirable dielectric characteristics.

 