A green body ceramic matrix composite material (30) is formed using
ceramic fibers (32) in an intermediate state disposed in a green body
ceramic matrix material (34). The fibers may be in either a dry but
unfired (green) condition or in a partially fired condition. Selective
control of the degree of pre-firing (pre-shrinkage) of the fibers may be
used to control the level of residual stresses within the resulting
refractory material resulting from differential shrinkage of the fibers
and the matrix material during processing of the composite material.