Method for refining and homogeneously distributing alloying partners and
for removing undesired reaction products such as oxides and/or slag in or
from soft solder during the production of fine solder powder, in which
the solder alloy is melted in a high temperature-resistant plant and/or
animal oil, the melt is moved to another container of oil with a
temperature of at least 20.degree. C. greater than the liquidus
temperature, stirred there, and subjected to multiple shear treatments
using rotors and stators for forming a dispersion comprising solder balls
and oil, from which dispersion the solder balls are separated by means of
subsequent sedimentation.