An improved seed/AFM structure is formed by first depositing a layer of tantalum on the lower shield. A NiCr layer is then deposited on the Ta followed by a layer of IrMn. The latter functions effectively as an AFM for thicknesses in the 40-80 Angstrom range, enabling a reduced shield-to-shield spacing.

 