There is provided a conductive curable resin composition comprising (A) a
curable resin composition comprising an elastomer with a Mooney viscosity
(ML.sub.1+4 (100.degree. C.)) of 25 or greater at 2-80 wt % and (B) a
carbon material, with a weight ratio of component (A) to component (B) of
70-5:30-95. The curable resin composition of component (A) preferably
comprises (A1) an elastomer at 80-2 wt %, (A2) a radical reactive resin
at 20-98 wt % and (A3) an organic peroxide at 0.2-10 parts by weight to
100 parts by weight of (A1+A2). Also provided are a process for
production of a conductive cured resin by shaping and curing of the
conductive curable resin composition, and a fuel cell separator, an
assembly for a cell, an electrode or a heat releasing plate, obtained
thereby.