The present invention provides a thermoplastic polyurethane composition which comprises an ethylene-vinyl alcohol copolymer and/or a polyamide, and a thermoplastic polyurethane, in which the retention of melt tension thereof, when kept in a molten state at 220.degree. C. for 1 hour, determined by the following equation (1), is not less than 10%. Retention of melt tension (%)=[Melt tension after being kept in a molten state/Melt tension before being kept in a molten state].times.100 (1)The thermoplastic polyurethane composition of the present invention is excellent in production stability of a molded article, and can provide a molded article excellent in appearance because the progress of gelation thereof is suppressed even in a molten state.

 