A method of manufacturing water-treatment particles comprises respectively
preparing a particle-fabricating solution that comprises chitinous
composition and a forming solution first. Next, a complex solution is
prepared by adding calcium sulfite into the particle-fabricating
solution. Finally, the complex solution is pumped into the forming
solution to form water-treatment particles. In addition, water-treatment
particles manufactured by the method above are also disclosed in the
specification.