A photoresist pattern is formed on an insulating substrate so that it has
a reverse tapered cross section and a reverse pattern of a wiring pattern
to be formed. Next, a nanoparticles-containing ink is injected on a
wiring region using an inkjet system, followed by a leveling process, a
drying process, a resist separation process and a baking process. Thus a
wiring pattern is formed.