A conductive composition comprises a poly(arylene ether), a polyamide, a conductive additive, and an impact modifier, wherein the composition demonstrates less than or equal to 0.0150 grams of composition buildup on the die face per minute of running time per meter of die opening perimeter after extruding the composition at a steady state for five minutes.

 