A clear thermoplastic blend comprises from about 25 to about 90 percent by weight of low flow polycarbonate resin having a MVR (Melt Viscosity Rate) of from about 1 to about 7 cc/10 min at 300.degree. C./1.2 kg and from about 10 to about 75 percent by weight of a polyester resin derived from the condensation of a cyclohexanedimethanol or equivalent thereof alone or with an ethylene glycol or equivalent thereof with a terephthalic acid or equivalents thereof or a combination of terephthalic acid and isophthalic acid or equivalents thereof.

 