The process of this invention involves first adsorbing a catalyst on the
surface of a specimen by immersion in a catalyst-containing solution,
followed by electrolytic deposition in a second solution that need not
contain catalyst. This two-step superconformal process produces a
seam-free and void-free metal microelectronic conductor.