An amorphous polyester chip having superior processing ability is characterized by a moisture content of not more than 300 ppm and a fine particle content of not more than 500 ppm. A preferred embodiment is a copolymerized polyester chip comprising a main repeating unit consisting of ethylene terephthalate, and 1,4-dimethylene-cyclohexane terephthalate or neopentyl terephthalate, wherein the glycol component of the copolymerized polyester has a specific composition of 50 to 85 mol % of ethylene glycol, 12 to 45 mol % of 1,4-cyclohexanedimethanol or neopentyl glycol and 1.5 to 7.0 mol % of diethylene glycol. Such amorphous polyester chip can be obtained by cooling an amorphous polyester obtained by melt polymerization, cutting the polyester to give a chip, feeding the chip in a treatment tank, drying the chip and removing fine particles.

 