A shrink film comprising a polyethylene film, characterized in that said polyethylene is an ethylene copolymer mixture having a molecular weight distribution in the range 10 to 35, a density of 915 to 940 kg/m.sup.3, a weight average molecular weight of at least 100000 D and an MFR.sub.2.16 (190.degree. C.) of 0.1 to 0.9 kg/m.sup.3, which copolymer mixture is produced by a two or more stage copolymerization of ethylene and 2 to 10% mole (relative to ethylene) of a C.sub.3-12 alpha-olefin comonomer in a series of reactors including at least one slurry loop reactor and at least one gas phase reactor using a heterogeneous Ziegler-Natta catalyst.

 